Commonly used to enrich the surface carbon content of steel that case hardening provides. This is intended to produce a high-hardness, wear-resistant surface supported by a tenacious core.
Steel 18CrNiMo7-6
CHARACTERISTICS
Medium hardenability steel that will achieve high strength levels after case hardening. It is ideal for parts that require core mechanical resistance in the 80 120 Kgf/mm2 (800-1200 MPa or N/mm2) range.
APPLICATIONS
Used to fabricate large or medium size gears, and pinion shafts for reducers.
SIMILAR MATERIALS
DIN WNr (1.6587)
Chemical Composition (% BY WEIGHT)
C
Mn
P
S
Si
Ni
Cr
Mo
V
0,15 – 0,21
0,50 – 0,90
0,035
0,035
0,40
1,40 – 1,70
1,50 – 1,80
0,25 – 0,35
-
THERMAL TREATMENT AND PROCESSING TEMPERATURES (°C)